HDPE Geomembrane pond Liner 2.0 thickness
HDPE Geomembrane liner are made from polyethylene polymer materials that blow molding,its main function is to prevent the liquid leakage and gas volatile.According to the production of raw materials can divide into HDPE geomembrane liner and EVA geomembrane liner,etc.
Geomembrane and Geotextile are widely used in lining of pond reservoirs, canal, waste water, landfill, a dams, Lakes and many other areas Due to cost effectiveness and resistance against chemical and weather conditions.
Main Features
Good mechanical propertiesHigh tear strength, deformation and adaptable, puncture resistance, anti-aging, anti-ultraviolet-resistant
Anti oil and salt, pH, anti-corrosion, high temperature-resistant, non-toxic, long service life. water, drainage, seepage, the good effect of moisture, width, thickness of the full range of specifications and low cost, simple construction.
Products Feature
1.Good physical and mechanic performance.
2.High tearing resistance, strong deformation adaptability.
3.Puncture-resisting, aging resisting, ultra-violet radiation, oil and salt, and corrosion resistance.
4.Good adaptability to high and low temperature, non-toxicity, long service life.
5.Good waterproof, drainage, anti-seepage and damp proof effects.
6.Complete width and thickness specifications, low cost and easy installation.
7, Apply to road construction, river levee, lake dam, sewage dam/ waste water dam, channel, liquid storage pool, metro, basement, tunnel, foundation, waste storage, marifarm/seawater farms, freshwater fish farm, /fishpond / aquatic farm, road, high way, expressway/motorway,
railway, roofing, and so on.
Technical Index
Thickness | 0.75 | 1.0 | 1.25 | 1.50 | 2.00 | 2.50 | 3.00 |
Density g/m2 | ≥0.94 | ≥0.94 | ≥0.94 | ≥0.94 | ≥0.94 | ≥0.94 | ≥0.94 |
Tensile yield strength (N/mm) | ≥11 | ≥15 | ≥18 | ≥22 | ≥29 | ≥37 | ≥44 |
Tensile breaking strength (N/mm) | ≥20 | ≥27 | ≥33 | ≥40 | ≥53 | ≥67 | ≥80 |
Bongation at yield(%) | ≥12 | ≥12 | ≥12 | ≥12 | ≥12 | ≥12 | ≥12 |
Elongation at break(%) | ≥700 | ≥700 | ≥700 | ≥700 | ≥700 | ≥700 | ≥700 |
Tear resistance(N) | ≥93 | ≥125 | ≥160 | ≥190 | ≥250 | ≥315 | ≥375 |
Puncture strength(N) | ≥240 | ≥320 | ≥400 | ≥480 | ≥640 | ≥800 | ≥960 |
Tensile load stress cracking | ≥300 | ≥300 | ≥300 | ≥300 | ≥300 | ≥300 | ≥300 |
Carbon black content(%) | 2.0-3.0 | 2.0-3.0 | 2.0-3.0 | 2.0-3.0 | 2.0-3.0 | 2.0-3.0 | 2.0-3.0 |